Smelted my first silver ingot :-) just need to get some forms to pore the smelt in for a better form. I had to use wet sand and make my own form but it worked.
Not sure don't have a scale. I had found it doing some prospecting in SD deadwood with my garret in . Had a lot of impurities it was alot of learning how to break it down and smelt it the right way. It's about 3" wide 31\4 long buy an inch thick. But trying to make a good deep square form out of wet sand to pore it in is well. You know lol it was a pretty good nugget.